ababy sharon on wed 11 aug 99

Hi!
It was like a miracle,that when we bought our new computer,I got the last
(or one before)CM,with an interesting article about glaze software's.CM July
Ougust98 Page38-42.
I tried some sophtwares.For a long time I worked with the Glaze
Simulator:This program is friendly to the person who does not understand too
much about computers&chemistry. It simulates the glazes situation but some
of the graphs are not clear.For me this program was an easy way to glaze
understudying.
It has some limits but it is easy to handle.
I moved to Insight, It was hard for me to learn partly,because of the
language and partly because I expected to know without learning. Anyway I
work with Insight and happy
it is a compact yet wide program!
....And more you read at CM

Ababi