search  current discussion  categories  forms - tiles 

clay for tiles in au

updated sun 22 aug 99

 

STEVE HOWKINS on sat 21 aug 99

Katie,

I made some thin 100m sq tiles recently. I used Clayworks WTB and fired to
cone 6.

There was no curling etc they all dried and fired flat. I did not put any
weights on them.

Regards Steve Howkins, Melbourne.