search  current discussion  categories  glazes - crazing & crackle 

turquoise crackle raku glaze

updated sun 5 sep 99

 

Karen Shapiro on fri 3 sep 99

Hi Clayarters,

I have a commission to do which calls for a beautiful clear turquoise (the
color of Windex). Anyone have any suggestions before I start testing in the
dark?