search  current discussion  categories  kilns & firing - cones & controllers 

malfunctioning cones

updated thu 9 sep 99

 

Bruce Girrell on wed 8 sep 99

Just wondering...

Has anyone who has had anomalous cone melting ever saved the cone pack and
sent it to Orton?

Someone here recently was talking with Orton by telephone about this
problem. Wouldn't it be helpful to them if they got some hard evidence of
the problem? They might even be able to analyze the cones to see what the
problem is/was.

Bruce "just a thought" Girrell