I have just found a great pair of UV blocking glasses that allows me to see
the flames at the burner as well in the kiln. Put out by Oberon Co. P O Box
N-1008 NewBedford, Mass 02746 1-800-face-fit .........#311-65 Tan
frame/Didymium II Lens with sideshields meets ANSI Z87.1 Used by lampworks
crafts people. I got mine at the Bookstore at Penland school $39 ......
Contact "Kat" at kat@m-y.net. I got the last 2 pair for friends but they
will have some in soon. Tracy