Eydie DeVincenzi on sun 19 sep 99
------------------
I do not remember who suggested using Future Clear Wax on pots in lieu of
glaze or burnishing, but THANK YOU=21
I have been looking for a substitute for a =5E6 clear glaze for my nerikome
pots. The glazes I've tried are so shiny that they distract from the
intricacies of my colored clay patterns that I spend so-o-o much time
developing.
The Future wax puts a lovely sheen on the surface of the piece, so it looks
'finished but not glossy.
Thanks again.
Eydie DeVincenzi
| |
|