OK, believe me I do not work for
Highwater, or own any stock. LOL
I just haven't had a need to try any
other supplier. For large sculptural
pieces(nothing life size, yet) I use
their Craggy Crunch. They use three
sizes of grog (19=25 total).
I have had great success with my
large pieces. Especially in the building
stages. And I have yet to have a piece
crack. So far I have fired it only in
my electric kiln. Highwater says it
does extremely well in wood fired kilns.
Sheron