Nan Smith on tue 28 sep 99

Dear Curt:

I wanted to add that I also wedge in a pinch of 1/2 inch chopped nylon per
grapefruit sized ball of clay. Please add this after mixing the recipe.

Nan
Nan Smith, Professor