search  current discussion  categories  materials - misc 

vinegar and glazing

updated fri 8 oct 99

 

arlene h. on wed 6 oct 99

I am wondering if vinegar irregularly spilt on greenware will have any
effect on the glazing result. For example: when attaching a handle and the
vinegar drips around the area. Will it just burn off without further
consequence? Thanks!

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com

Peggy Dalberto on thu 7 oct 99

Hi, I use vinegar all the time for handles, never seems to affect the
quality of the glaze. I can't imagine it surviving the bisque firing. If
in doubt, sacrifice something.
----- Original Message -----
From: arlene h.
To:
Sent: Wednesday, October 06, 1999 2:03 PM
Subject: vinegar and glazing


> ----------------------------Original message----------------------------
> I am wondering if vinegar irregularly spilt on greenware will have any
> effect on the glazing result. For example: when attaching a handle and
the
> vinegar drips around the area. Will it just burn off without further
> consequence? Thanks!
>
> ______________________________________________________
> Get Your Private, Free Email at http://www.hotmail.com
>