search  current discussion  categories  glazes - misc 

willendorf glaze

updated fri 15 oct 99

 

Michele Jurist on thu 14 oct 99

To the person requesting the Willendorf glaze. I found this recipe in my
files, don't know if this is what you are looking for. I have never used it
before, and I can only guess that the cone is 04, since most of my recipes
fire in that range.

Hope this helps.

Willendorf (Not for dinnerware -- toxic)

Frit 3304 51.7
EPK 26.1
Lithium Carbonate 22.2

Add 2% chrome.

Michele