search  current discussion  categories  kilns & firing - misc 

firing temp for willendorf glaze

updated sat 16 oct 99

 

Priscilla Hollingsworth on fri 15 oct 99

To get the most disgusting/exciting reds and oranges from the Willendorf
glaze, I found that I needed to fire it to 09 - 010. Cone 04 was too
high.