Craig Fulladosa on sat 16 oct 99
I am wanting to experiment with screen printing some tiles with an ink
for tiles witch consists of medium to heavy bit of mineral oil with
manganese oxide witch will serve as a borderline for glazing in
different colors I think it may have been called the, cuerda seca effect
on tiles. If you know how to do this or know where I can learn more
about it please let me know. I would like to minimize time in
testing out this idea. Thanks.
--
Craig