Sheron Roberts on sun 31 oct 99

------------------
Hi everyone,
I have just gone through the
fun task of salvaging files,
reformatting and restoring my
hard drive. My modem
disappeared, or so my
computer kept telling me.
So no email access
for 2 weeks.
I have a copy of Electric Kiln
Ceramics, second edition.
I mixed the Franklin R 92
glaze straight from the book
and it came out exactly like the
book stated. A really nice glaze.
I like the descriptions given for
each glaze.
Sheron in NC