search  current discussion  categories  materials - misc 

the cadmium thread

updated sat 13 nov 99

 

Lesley Alexander on fri 12 nov 99

As reported a few months ago, I used thick cadmium-encapsulated stains on
a bowl, covered with a very light coat of clear. It tested OK when I sent
it to Alfred.
If I wanted to use a glaze with a % of cadmium, I'd do a test bowl with
the glaze plain, and one with a light coating of clear over the glaze, and