k200 feldspar?

updated tue 16 nov 99

 

Judy Musicant on sat 13 nov 99

I have a bag of F-4 Kona Feldspar that also has a large 200 printed on it.
It's a soda feldspar. Could that be the same or similar to the K200
Feldspar mentioned earlier?

Judy

Ron Roy on mon 15 nov 99

Kona F4 is a soda spar - probably 200 mesh.

K200 is a potash spar

They are not the same but some glazes will work with either.

RR