mel jacobson wrote:

> the one thing i have discovered, what old delkic came up with does work.
> i have been sent samples of several new products to spray on kilns ( made
> by big ceramic companies), have not done it yet. do not have a new kiln
> to spray, but will in time. obviously others are testing ideas.

Mel,
Just found this old message by accident. Would it work for testing purposes to
spray these new substances on freestanding bricks, then put these bricks in say
the lowest part of the kiln on a shelf by themselves, to test for this spalling
stuff?
Just a thought.....

Lisa (whose server has been holding back mail, about 6 million bytes worth)