Gus Morcate on sun 5 dec 99

Metallic Black
Kaolin 95
Soda Feldspar 1526
Whiting 106
Gersley Borate 208
Copper Carb. 80
Cobalt Carb. 40

White Gloss
Kaolin 270
Flint 160
Frit 3134 490
Tin Oxide 80

Bean Pot Brown
Frit 3134 200
Dolomite 200
Spodumene 200
Ball Clay 200
Flitnt 200
Tin Oxide 50
Red Iron Oxide 40

Gloss Dark Blue
Gersley Borate 500
Kaolin 150
Flint 350
Cobalt Carb. 20

Antique Green
Kaolin 270
Flint 160
Frit 3134 490
Tin Oxide 80
Copper Carb. 20
Red Iron Ox. 20

Robins Egg
Flint 56
Whiting 188
Soda Feldspar 516
Kaolin 154
Zinc Oxide 86
Copper Carb. 20
Rutile 40

Dave's Blue
Kaolin 270
Flint 160
Frit 3134 490
Tin Ox. 80
Cobalt Carb. 2.5
Copper Carb. 10

Barium Mat
Nepheline Syenite 600
Barium Carbonate 240
Lithium Carbonate 50
Kaolin 60
Flint 50
Copper Carb. 30

Metallic Green
Ball Clay 60
Dolomite 180
Gersley Borate 220
Spodumene 360
Tin Oxide 80
Zircopax 100
Copper Carb. 60

Moondust
Soda Feldspar 330
Wollastonite 300
Ball Clay 250
Zinc Oxide 120
Rutile 50

Speckled White
Gersley Borate 500
Kaolin 200
Flint 300
Zircopax 100
Rutile 50

Eggshell Blue
Wollastonite 350
Soda Feldspar 350
Ball Clay 390
Zinc Oxide. 140
Cobalt Carb. .6
Rutile 4

Stonehenge
Flint 56
Whiting 188
Soda Feldspar 516
Kaolin 154
Zinc Oxide 86
Rutile 40
Ilmenite(add after sieving) 30
Cobalt Carb. 10

Mint Mist
Kaolin 270
Flint 160
Frit 3134 490
Tin Oxide 80
Copper Carb. 20

Blue Brown
Custer Feldspar 455
Whiting 236
Ball Clay 218
Zinc Oxide 91
Flint 91
Cobalt Carb. 20
Rutile 40
Red Iron Oxide 20

Morgans Tan
Kaolin 270
Flint 160
Frit 3134 480
Tin Oxide 80
Red Iron Oxide 30
Rutile 40
Mady's Mat
Soda Feldspar 500
Whiting 100
Kaolin 200
Zinc Oxide 100
Talc 150
Cobalt Carb. 2.5
Copper Carb. 10

Asako White
Flint 56
Whiting 188
Soda Feldspar 516
Kaolin 154
Zinc Oxide 86
Rutile 40
Ilmenite 30
add Ilmenite after sieving

Jade Green
Gersley Borate 900
Flint 585
Kaolin 315
Coper Carb. 72

Bahamas Blue
Nepheline Syenite 470
Gersley Borate 270
Flint 200
Kaolin 50
Red Iron Oxide 20
Cobalt Carb. 15
Rutile 40

Floating Blue
Nepheline Syenite 473
Gersley Borate 270
Flint 203
Kaolin 56
Red Iron Ox. 20
Cobalt Carb. 20
Rutile 40
Bentonite 11