search  current discussion  categories  glazes - misc 

a new addition to the glaze family

updated mon 13 dec 99

 

Sarah Lackey on thu 9 dec 99

Evenin'!

I discovered a glaze while attempting to recreate the result of a mixture of
tests. It's a lovely grey with metallic highlights. Pictures of it and the
recipe formula are at
http://www.fortunecity.com/greenfield/runningbrook/455/grey.html I hope you
all enjoy it as much as I have. I'm testing some pots overlapping that and
the Kemp 17 red. Now my problem is patience while waiting on the kiln.

Sarah in Tennessee
Who has mysteriously started to live, eat and breathe pottery in the last
year or so.

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com

Andi Cody on fri 10 dec 99

Hi Sarah,

What cone do you fire this to?

At 11:19 AM 12/09/1999 EST, you wrote:
>----------------------------Original message----------------------------
>Evenin'!
>
>I discovered a glaze while attempting to recreate the result of a mixture of
>tests. It's a lovely grey with metallic highlights. Pictures of it and the
>recipe formula are at
>http://www.fortunecity.com/greenfield/runningbrook/455/grey.html I hope you
>all enjoy it as much as I have. I'm testing some pots overlapping that and
>the Kemp 17 red. Now my problem is patience while waiting on the kiln.
>
>Sarah in Tennessee
>Who has mysteriously started to live, eat and breathe pottery in the last
>year or so.
>
>______________________________________________________
>Get Your Private, Free Email at http://www.hotmail.com
>


thanks,

Andi

email: mailto:acody@ucsd.edu

Sarah Lackey on sun 12 dec 99


Cone 6. . .oxidation. . .sorry bout that!

Sarah

>From: Andi Cody
>Reply-To: Ceramic Arts Discussion List
>To: CLAYART@LSV.UKY.EDU
>Subject: Re: a new addition to the glaze family
>Date: Fri, 10 Dec 1999 13:39:54 EST
>
>----------------------------Original message----------------------------
>Hi Sarah,
>
>What cone do you fire this to?
>
>At 11:19 AM 12/09/1999 EST, you wrote:
> >----------------------------Original message----------------------------
> >Evenin'!
> >
> >I discovered a glaze while attempting to recreate the result of a mixture
>of
> >tests. It's a lovely grey with metallic highlights. Pictures of it and
>the
> >recipe formula are at
> >http://www.fortunecity.com/greenfield/runningbrook/455/grey.html I hope
>you
> >all enjoy it as much as I have. I'm testing some pots overlapping that
>and
> >the Kemp 17 red. Now my problem is patience while waiting on the kiln.
> >
> >Sarah in Tennessee
> >Who has mysteriously started to live, eat and breathe pottery in the last
> >year or so.
> >
> >______________________________________________________
> >Get Your Private, Free Email at http://www.hotmail.com
> >
>
>
>thanks,
>
>Andi
>
>email: mailto:acody@ucsd.edu

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com