Sarah Lackey on thu 9 dec 99
Happy Christmas everyone!
Thanks for all the red glaze recipes. They're all fantastic and I had a
horrendous time trying to pick one to use. Kemp's 17 won out though. It
turned a lovely kind of translucent wine color with bluish/purple opalescent
streaks in the thick spots.
That burgundy satin is great too. It turned a nice brick color that looked
like someone sprinkled black pepper all over it. I used Custer instead of
G-200 (necessary roughness).
I'll be doing much more red testing after Christmas, I can tell that
already. Thanks again everyone!