In a message dated 12/8/99 9:46:53 AM Pacific Standard Time, ronroy writes:

> See above comments for Bahamas Blue - the bentonite is there to help
> counteract the reology problems.

Could you tell us what "reology" means? Is this a new science?

Milton NakedClay@AOL.COM

Yucca Valley, CA Cloudy and chilly, but the air is still. Possibly the calm
before the expected storm.

Gregory D Lamont on sun 12 dec 99

At 06:17 PM 12/10/99 -0500, you wrote:
>----------------------------Original message----------------------------
>In a message dated 12/8/99 9:46:53 AM Pacific Standard Time, ronroy writes:
>
> > See above comments for Bahamas Blue - the bentonite is there to help
> > counteract the reology problems.
>
>Could you tell us what "reology" means? Is this a new science?
>
>Milton NakedClay@AOL.COM
>
>Yucca Valley, CA Cloudy and chilly, but the air is still. Possibly the calm
>before the expected storm.

Hi Milton,

"Reology" should have been written "rheology" and is, according to Funk and
Wagnall's, " ... the study of the properties and behavior of of flowing
substances; the science of flow."

Happy Holidays
Greg

gdlamont@iastate.edu
http://www.ourwebpage.net/greglamont/

Mailing address:
Greg Lamont
3011 Northwood Drive
Ames, IA 50010-4750
(515) 233-3442

Ron Roy on sun 12 dec 99

Reology is the study (correct me if I am not explaining this correctly
anyone) of solids in suspension I think - in our case it has to do with
slip density, flow time, viscosity - like that - and how to alter those
properties. It would be applicable to flocculating or deflocculation of
slips and glazes.

RR

>----------------------------Original message----------------------------
>In a message dated 12/8/99 9:46:53 AM Pacific Standard Time, ronroy writes:
>
>> See above comments for Bahamas Blue - the bentonite is there to help
>> counteract the reology problems.
>
>Could you tell us what "reology" means? Is this a new science?
>
>Milton NakedClay@AOL.COM
>
>Yucca Valley, CA Cloudy and chilly, but the air is still. Possibly the calm
>before the expected storm.

Ron Roy
93 Pegasus Trail
Scarborough
Ontario, Canada
M1G 3N8
Evenings 416-439-2621
Fax 416-438-7849