search  current discussion  categories  glazes - crazing & crackle 

white crackle glaze

updated tue 21 dec 99

 

Wade Blocker on mon 20 dec 99



----------
> From: Wade Blocker
> To: clayart@lsv.uky.com
> Subject: white crackle glaze
> Date: Thursday, December 16, 1999 9:23 PM
>
> Ellen,
>
> The following glaze is from Daniel Rhodes. I have used it over porcelain,
> it is a great crackle glaze.
>
> White opaque crackle glaze cone 9-l0
>
>
> Cornwall Stone 85
> Whiting l5
>
> Mia in ABQ