Peter Atwood on fri 24 dec 99
Hi Mel,
I have tested HiHO SIlver on a white burning stoneware body and got a
beautiful pale yellow, almost a white with yellow tones. It was a nice
satiny surface. I believe it was fired in medium reduction to cone 9 ,maybe
as high as 10.
I bet this glaze will combine nicely with others but I haven't tested it any
more than just that once. A splash of Pete's Cranberry would be sweet. I
haven't seen it go to the silver color and am wondering what would cause
that effect. Would it be the claybody, the thickness of application, or just
the atmosphere? Hope you test it and let us know.
Peter Atwood