I've seen hi ho silver discussed several times, but have not seen the
formula.
I'd like to try the glaze. Would someone please send me the recipe so that
I can try the glaze in my situation on my clay? Thanks if you can help.
Baery in Westbank
email: baery@silk.net

Lesley Alexander on fri 31 dec 99

This is the recipe copied from Mel:

** Hi Ho Silver
cone 10
yellow to orange, to silver.
thin application.

nephy sy 60
dolomite 18 (slight change from original)
ball clay 15
tin 4
bentonite 3

this is from st.paul potter mike norman.
he thinks it is a western u.s. glaze.