search  current discussion  categories  kilns & firing - pit firing 

wince for pit fired porcelain

updated sat 22 jan 00

 

Russel Fouts on fri 21 jan 00

Ivor,

>> A long time ago an English pottery which was famous for its work, which
may have
been Bone China or Porcelain but it was vitrified (china) had an
advertisement which showed an elephant standing on cups and saucers. <<

John Chalke had a photo of a LONDON DOUBLE DECKER BUS resting on 4 porcelain
teacups. It was in an article in (I think) Ceramic Review about his recent
glaze experiments.

Russel

Russel Fouts
Mes Potes & Mes Pots
Brussels, Belgium
Tel: +32 2 223 02 75
Mobile: +32 476 55 38 75
Http://www.mypots.com
http://www.Japan-Net.ne.jp/~iwcat