say, i may have said this before.
i mix bentonite with water, mix it in a blender
then put it in a tight sealed container.
add it to a glaze wet...it disperses like a dream.
mel/mn
http://www.pclink.com/melpots (website)
from minnetonka, minnesota, u.s.a.

Stephen Mills on wed 2 feb 00

Possibly one of THE most important tools in a clay workshop is a
blender. I'd be totally lost...correction...totally knackered without
mine!!

Steve
Bath
UK


In message , mel jacobson writes
>----------------------------Original message----------------------------
> say, i may have said this before.
>i mix bentonite with water, mix it in a blender
>then put it in a tight sealed container.
>add it to a glaze wet...it disperses like a dream.
>mel/mn
>http://www.pclink.com/melpots (website)
>from minnetonka, minnesota, u.s.a.
>

--
Steve Mills
Bath
UK
home e-mail: stevemills@mudslinger.demon.co.uk
work e-mail: stevemills@bathpotters.demon.co.uk
own website: http://www.mudslinger.demon.co.uk
BPS website: http://www.bathpotters.demon.co.uk
Tel: **44 (0)1225 311699
Fax: **44 (0)870 0526466