Vince Pitelka on wed 2 feb 00
>I also wanted to thank you for your terra sig instructions. You sent them to
>me a couple years ago, and I only recently got around to trying them on some
>local red clay. You're right, you're right, you're right! It *is* magic.
> I thought you were being a bit, um, over-enthusiastic when
>you said a good terra sig was possibly the most perfect substance in
>existence, but now I agree with you. This is Cool!
I have already received several requests for insructions, as a result of
this very kind and flattering post. My thanks to Cindy Strnad for her
enthusiasm. To access my spiel on terra sig, go to Tony Hansen's IMC
website at http://digitalfire.com/education/glaze/terasig.htm
After you read that, email me if you have any questions.
Best wishes -
- Vince
Vince Pitelka
Home - vpitelka@DeKalb.net
615/597-5376
Work - wpitelka@tntech.edu
615/597-6801 ext. 111, fax 615/597-6803
Appalachian Center for Crafts
Tennessee Technological University
1560 Craft Center Drive, Smithville TN 37166
| |
|