Does anyone have the proper conversion from gerstley borate to frit 3134? Thanks.. Marshall http://www.potteryinfo.com/cgi-bin/potterycgi/Ultimate.cgi?action=intro
------------------- Frit 3134 0.316 Na2O 0.684 CaO 0.632 B2O3 1.47 SiO2 Gerstley Borate 2 CaO 3 B2O3 5 H2O As you can see there=92s not a direct substation here if that=92s your?