Vince volunteered:
> You
> should not need to screen the glaze unless there are big lumps in it. I
> recommend getting a fairly fine small-size kitchen strainer, and run the
> glaze through that when you pour it in the spray-gun reservoir.
>
Talisman makes a very nice small test sieve that fits will in quart
yogurt etc. containers. They come in varying meshes, and last time I
checked the test sieves were about $8.00 at Highwater Clay. VERY handy
for screening small amounts of liquids.
--