updated wed 16 feb 00

 

Jack & Peggy on sun 13 feb 00

-------------------
My buddy fires an updraft kiln at earthenware temps. and is way back =22in
country=22, and is having big trouble with uneven firings. I haven't any
experience with this type kiln and can't help him. What can he do to check =
for
proper operation without losing pots?

Norman van der Sluys on tue 15 feb 00

It would help to know a little more about his kiln. He should try to distribute
the mass in the kiln evenly and not fire too fast. Also the exit flue might be
open too far.

Norman van der Sluys



Jack & Peggy wrote:

> ----------------------------Original message----------------------------
> -------------------
> My buddy fires an updraft kiln at earthenware temps. and is way back "in
> country", and is having big trouble with uneven firings. I haven't any
> experience with this type kiln and can't help him. What can he do to check for
> proper operation without losing pots?