search  current discussion  categories  glazes - cone 4-7 

^6 porcelain

updated wed 16 feb 00

 

Paul Jadick on tue 15 feb 00

I must have tried every porcelain sold on the northeast coast from 6-10.
Now that I am working at ^6 oxidation I love the Standard #365 ^6 grolleg.
It is the best throwing of any I have tried and so far no trouble with
bloating. I bisque slowly (with my students work) and I soak my glaze
firings.. It ends up a high ^6. So far so good.

Georgia Tenore
pjadick@worldnet.att.net