correction: re:need glaze recipe call yellow salt

updated wed 16 feb 00

 

Bonita Cohn on tue 15 feb 00

OOPS! CORRECTION!!!SORRY!
In This recipe I left out the Silica (Don't you do that!)
Biz Littell's Yellow-yellow green glaze cone 10-11
Kaolin 10
whiting 8
Talc 15
flint 30
custer spar 37
100
plus: iron oxide 10%