Hi- We make our cabinet knobs/pulls in both =5E6 stoneware and =5E6 =
porcelain by
throwing them off the hump, solid clay, right side up. When they are still =
damp
They are turned over and trimmed slightly to make sure they are flat on the
bottom=3B and then a hole is=22drilled out =22 with a trimming tool. I found=
excellent
glue in hardware from Axner Ceramic Supply in Florida at an excellent price.
Saves a lot of guess work finding the right size parts at the hardware =
store.
Good luck with your project=21-Kathy Chase