Deborah Bouchette on sat 11 mar 00
------------------
I use my kiln for glass fusing and love it. Please see my web site,
www.aleatoric-art.com, which has a fusing chart and all sorts of data about
firing glass in an electric kiln.
Deb Bouchette
-----Original Message-----
From: Judy Hitchens =5BSMTP:sweetpea=40auracom.com=5D
Sent: Wednesday, March 08, 2000 2:41 PM
Subject: use of pottery kiln for glass
----------------------------Original message----------------------------
Hi :) I was wondering whether anyone has used their pottery kiln for
various glass procedures. I understand from a kiln manufacturer that this
is possible though results may not be as predictable as with a glass kiln.
Thanks for any answers.
Cheers from Nova Scotia,
Judy
| |
|