Sharon31 on fri 17 mar 00
Hi!
This question is to European - ClayArter!
What is the highest temerature I can bisque WBB Vingerling K 129 and still
get a nice Raku glaze ^08-^05?
Ababi
sharon@shoval.org.il
http://www.israelceramics.org/main.asp?what=gallery
http://clay.justnet.com/cgallery/asharon.htm
Marie-Claire Stil on wed 22 mar 00
------------------
On Fri, 17 Mar 2000 12:22:30 EST, you wrote:
=3E----------------------------Original message----------------------------
=3EHi=21
=3EThis question is to European - ClayArter=21
=3EWhat is the highest temerature I can bisque WBB Vingerling K 129 and =
still
=3Eget a nice Raku glaze =5E08-=5E05?
=3EAbabi
=3Esharon=40shoval.org.il
=3Ehttp://www.israelceramics.org/main.asp?what=3Dgallery
=3Ehttp://clay.justnet.com/cgallery/asharon.htm
Hi Ababi
The highest temperature for this clay is 1280c, but I would'nt bisque
that high for raku because the glaze would not adhere the same way
than with lower bisque.
I suppose you usually bisque higher than glaze stoking?
Have fun,
Marie Claire (trying to catch up with Clayart)
| |
|