search  current discussion  categories  materials - gerstley borate 

raku glazes-no gerstley

updated mon 10 apr 00

 

skhouse@excite.com on thu 6 apr 00


I will be teaching a workshop in a week or so and was hoping for a few more
Raku glazes that do not contain Gerstley Borate. i hope to have enough for a
few old favorites, but i think there is less than 10 lbs. left. If anyone
has any good recipies please send them to me. I and my students will be
grateful although most are beginners and will not know it.
Sarah House
skhouse@excite.com





_______________________________________________________
Get 100% FREE Internet Access powered by Excite
Visit http://freelane.excite.com/freeisp

Anji Henderson on sat 8 apr 00

I havn't done this but I was told.... The copper spray
paint and silver and aw, heck one other color.. I
don't remember what the other color is.. Well any way
I was told that it makes bueatiful things happen in
the reduction of raku.. And I was told that it can
stand alone..

Now did I add enough disclaimers if it is not true
and/or if it dosn't work?? :) But heck I am game and
when I get caught up with this yard.....
Hahahahahahahaahahahaa (oh my one is never really
caught up) I can get on with raku-ing and give it a
try my self...

Anji
-- Spent 4 hours in the yard and only have the front
done... Arrugh... gotta trim... Hahahahahaha
Everything!!! (clay and yard)

--- skhouse@excite.com wrote:
> ----------------------------Original
> message----------------------------
>
> I will be teaching a workshop in a week or so and
> was hoping for a few more
> Raku glazes that do not contain Gerstley Borate. i
> hope to have enough for a
> few old favorites, but i think there is less than 10
> lbs. left. If anyone
> has any good recipies please send them to me. I and
> my students will be
> grateful although most are beginners and will not
> know it.
> Sarah House
> skhouse@excite.com
>
>
>
>
>
>
_______________________________________________________
> Get 100% FREE Internet Access powered by Excite
> Visit http://freelane.excite.com/freeisp
>

__________________________________________________
Do You Yahoo!?
Talk to your friends online with Yahoo! Messenger.
http://im.yahoo.com

Earl Brunner on sun 9 apr 00

Ok, one other disclaimer, you probably want to put the spray
paint on
the pot BEFORE firing, not as it comes out of the kiln?
Some of those
aerosols can be quite flammable.

Anji Henderson wrote:
>
> ----------------------------Original message----------------------------
> I havn't done this but I was told.... The copper spray
> paint and silver and aw, heck one other color.. I
> don't remember what the other color is.. Well any way
> I was told that it makes bueatiful things happen in
> the reduction of raku.. And I was told that it can
> stand alone..
>
> Now did I add enough disclaimers if it is not true
> and/or if it dosn't work?? :) But heck I am game and
> when I get caught up with this yard.....
> Hahahahahahahaahahahaa (oh my one is never really
> caught up) I can get on with raku-ing and give it a
> try my self...
>
> Anji
> -- Spent 4 hours in the yard and only have the front
> done... Arrugh... gotta trim... Hahahahahaha
> Everything!!! (clay and yard)
>
> --- skhouse@excite.com wrote:
> > ----------------------------Original
> > message----------------------------
> >
> > I will be teaching a workshop in a week or so and
> > was hoping for a few more
> > Raku glazes that do not contain Gerstley Borate. i
> > hope to have enough for a
> > few old favorites, but i think there is less than 10
> > lbs. left. If anyone
> > has any good recipies please send them to me. I and
> > my students will be
> > grateful although most are beginners and will not
> > know it.
> > Sarah House
> > skhouse@excite.com
> >
> >
> >
> >
> >
> >
> _______________________________________________________
> > Get 100% FREE Internet Access powered by Excite
> > Visit http://freelane.excite.com/freeisp
> >
>
> __________________________________________________
> Do You Yahoo!?
> Talk to your friends online with Yahoo! Messenger.
> http://im.yahoo.com

--
Earl Brunner
http://coyote.accessnv.com/bruec
mailto:bruec@anv.net