Sharon31 on mon 10 apr 00
Thre was a mistake in the earlier letter
Frit 6004
=============
Na2O................ 11.50 11.50%
Al2O3............... 3.50 3.50% *****
K2O................. 15.50 15.50%*****
Si2O3............... 44.00 44.00%
B2O3................ 25.50 25.50%