Tony Hansen on fri 14 apr 00
We should be sampling 'BORAQ Plastic Borate' in a few weeks. Don't email
me personally but I'll notify the list where to get it. Samples will be
available on an
ecommerce website with online support and information on how to use it
plus an email newsletter. We'll 'upgrade' the formula to improve it as we get
feedback from users (we cannot do this alone). Thanks to those who sent
their glaze recipes in for testing. I never really appreciated GB until we
lost it
but now that it appears a more consistent material can at least partially
replace it I am excited.
====================================================
T o n y H a n s e n thansen@digitalfire.com
http://digitalfire.com Calculation/Database Software for Ceramic Industry
http://ceramicsearch.com Search engine for the Ceramic Industry
--
Report our performance to The Public Eye at
http://208.8.12.151/addcomments.cfm?&key=3606
====================================================
T o n y H a n s e n thansen@digitalfire.com
http://digitalfire.com Calculation/Database Software for Ceramic Industry
http://ceramicsearch.com Search engine for the Ceramic Industry
| |
|