mel - hi ho silver cone 10 reduction glaze

updated sat 15 apr 00

 

Edward Cowell on fri 14 apr 00

Mel:

Love the smooth feel of this glaze as well as the variation in colour, but
have fine crazing upon closer examination. Added 4% fine silica and found
the crazing even more pronounced. I assume the problem is that this glaze
just doesn't fit my porcelain body.

Laurie Cowell,
Waterloo, Ontario, Canada

Edward Cowell on fri 14 apr 00


Mel:

Love the smooth feel of this glaze as well as the variation in colour, but
have fine crazing upon closer examination. Added 4% fine silica and found
the crazing even more pronounced. I assume the problem is that this glaze
just doesn't fit my porcelain body. Any suggestions on how I might alter
the glaze?

Laurie Cowell,
Waterloo, Ontario, Canada