search  current discussion  categories  techniques - throwing 

throwing miniatures

updated fri 12 may 00

 

Andie on fri 5 may 00

------------------
I would like to email with someone who has experience in throwing miniatures=
(1
1/2=22 or smaller). I'd like to get some advice about trimming my minis, and=
also
some glaze suggestions. If anyone works in small scale pottery, please email=
me
off list.

Thanks=21

Andie Carpenter



EMAIL: andiekc=40yahoo.com

OFFICIAL HOMEPAGE: www.andie.net

Andie on thu 11 may 00

------------------
I have gotten many, many emails requesting that I post a summary of the
responses that I got in this thread, as most of the responses I got were
off-line. I'm happy to do so, but as I got a couple dozen very detailed
responses, it will take me a couple days to summarize them.

In the meantime, one person who responded reminded me that the January 2000
Ceramics Monthly cover story was about a potter who throws tiny miniatures, =
and
when I dug it out, I found it had some really helpful step-by-step photos, =
and
great information. Thought I'd mention it, so maybe you guys could look =
through
that while I put together an extensive summary for the list.

: )

Andie



EMAIL: andie=40princessco.com

OFFICIAL HOMEPAGE: www.andie.net