search  current discussion  categories  glazes - cone 4-7 

[cone 6 glaze or slip with a copper penny look (shiny)]

updated wed 17 may 00

 

Deeclay@AOL.COM on mon 15 may 00


Also try Amaco Luster Gold L-518. It's an 04 glaze but put on 4 even coats
and it will go to cone 6 but looks great at cone 2.
Not copper but a nice old gold.
Diane in Miami

priddy on mon 15 may 00


Spectrum ^05 "bronze" and "pewter" go to ^7 with only a little running
and look fabulous



respectfully submitted,
elizabeth priddy