search  current discussion  categories  places - usa 

do you use mb stoneware from minnesota clay

updated mon 22 may 00

 

Ron Roy on sun 21 may 00


I am trying to solve a fit problem for someone using MB stoneware clay from
Minnesota Clay company.

They cannot answer the COE questions I have nor will they provide the names
of anyone using this body.

If you are using this clay - would you be so kind as to let me look at the
recipe of a glaze that fits it. I promise I will keep all information
confidential - just communicate with me directly at:

ronroy@total.net

Ron Roy




Ron Roy
93 Pegasus Trail
Scarborough
Ontario, Canada
M1G 3N8
Evenings 416-439-2621
Fax 416-438-7849