John & Anne Worner on tue 23 may 00
Hi all,
Ron Roy has gotten the oxide analysis from Laguna and it is
as follows:
Laguna Borate - May/00 - adjusted to add to 100 (99.9) with LOI
included.
Na2O - 3.97
K2O - 1.42
CaO - 18.86
MgO - 2.26
Al2O3 - 8.07
SiO2 - 18.75
B2O3 - 27.52
TiO2 - .07
Fe2O3 - .07
L.O.I. - 19.0
Total - 99.99
| |
|