In a message dated 5/23/00 11:50:38 AM, melpots@PCLINK.COM writes:

>my favorite glaze of all time for the electric kiln is a combination
>of gertsley borate and volcanic ash.
>
>i made a 60 ash, 40 volcanic...added about 3 percent zircopax..any
>colorant....and, instant glaze. like cone 5-6. high school kids loved
>it.

I guess you mean 60 percent ash and 40 GBorate?