Veena Raghavan on tue 30 may 00


Would someone enlighten me on what adhesive they use for lotion/ soap
dispensers??

-------------------------
Hi Robert,
I have been using E6000. It works for pumps most of the time. I
have had one or two people come back to have the pumps restuck, but this in
a period of five years or so, since I switched to E6000.
Hope this helps.
All the best.

Veena

Veena Raghavan
75124.2520@compuserve.com

Bob Hanlin on wed 31 may 00


I use E6000. You've got to be careful with it though, if you apply in and
then press the parts together they'll come apart. But...if you apply and
just set the collar on the clay piece gently and leave it 24 hours it'll
stay! And I mean stay!

BobH.

----- Original Message -----
From: "Veena Raghavan" <75124.2520@COMPUSERVE.COM>
To:
Sent: Tuesday, May 30, 2000 8:07 PM
Subject: Adhesive for soap/lotion pumps


> Would someone enlighten me on what adhesive they use for lotion/ soap
> dispensers??
>
> -------------------------
> Hi Robert,
> I have been using E6000. It works for pumps most of the time. I
> have had one or two people come back to have the pumps restuck, but this
in
> a period of five years or so, since I switched to E6000.
> Hope this helps.
> All the best.
>
> Veena
>
> Veena Raghavan
> 75124.2520@compuserve.com
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>

thansen@DIGITALFIRE.COM on thu 1 jun 00


--==__==__A8420XZ382__==__==
Content-Type: text/plain; charset="us-ascii"
Content-Transfer-Encoding: 7bit

> Would someone enlighten me on what adhesive they use for lotion/ soap
> dispensers??
> I have been using E6000. It works for pumps most of the time. I
> have had one or two people come back to have the pumps restuck, but this in
> a period of five years or so, since I switched to E6000.

You can get this at axner.com, just search for E-6000 (in
Materials/Equipment/Supplies). The search field is at the top of
the store home page.

--
====================================================
T o n y H a n s e n thansen@digitalfire.com
http://digitalfire.com Calculation/Database Software for Ceramic Industry
http://ceramicsearch.com Search engine for the Ceramic Industry

--



--==__==__A8420XZ382__==__==--