search  current discussion  categories  techniques - spraying 

spraying with out a compresser!!!

updated thu 1 jun 00

 

Anji Henderson on wed 31 may 00


A friend of mine showed me the coolest gadget.. It is
a Preval sprayer... I would not suggest trying to do
hundreds of mugs or anything, but for small stencils
or spray additions or even small works it is great..
It is at Home Depot or I suppose you can find it at
any hardware store.. Chanel B&G where ever I guess..
The can says it will spray at a 45 degre angle, an
sprays up to 16 oz of liquid... The whole set up is
about 3.00 and just the aresol part is like 2.00 ..
This is extra cool to me because I don't do major
spraying and it dosn't take up much room or money..

Anji

__________________________________________________
Do You Yahoo!?
Send instant messages & get email alerts with Yahoo! Messenger.
http://im.yahoo.com/

Kurt Wild on wed 31 may 00


Anji Henderson wrote:
>
> A friend of mine showed me the coolest gadget.. It is
> a Preval sprayer... I would not suggest trying to do
> hundreds of mugs or anything, but for small stencils
> or spray additions or even small works it is great..
> It is at Home Depot or I suppose you can find it at
> any hardware store.. Chanel B&G where ever I guess..
> The can says it will spray at a 45 degre angle, an
> sprays up to 16 oz of liquid... The whole set up is
> about 3.00 and just the aresol part is like 2.00 ..
> This is extra cool to me because I don't do major
> spraying and it dosn't take up much room or money..
>
> Anji

I found the Preval sprayer at an auto parts store (Carquest).

Kurt Wild
1000 E. Cascade Ave.
River Falls, WI 54022
Phone: 715-425-5715
email: KURT.L.WILD@UWRF.EDU
web site: http://wwwpp.uwrf.edu/~kw77/