microcrystalline wax.

updated sat 3 jun 00

 

iandol on fri 2 jun 00


Subject: wax

Millie,

I found my Microcrystalline Wax at the Arts and Crafts Shop. It is sold =
for the people who do Batik. Because it has a high melting point it =
tends to be brittle when cold. So those people who like lots of crazy =
lines in their dyed work mix it in with softer wax in varying degrees to =
control crackle patterns.

Hope that helps you trace the stuff.

Ivor Lewis.=20