Jim,
My raw material data base has the following information on your request
for an analysis of Frit 3289(Ferro).
Barium borosilicate frit.
Fusion at 1500F.
Similar frits: Pemco P-626, Fusion F-65.
Analyses:
Hopper:
% 5.5 Na2O 27.4 BaO 12.4 B2O3 5.4 Al2O3 49.3 SiO2
Cooper & Royle:
% 5.5 Na2O 27.4 BaO 12.4 B2O3 5.4 Al2O3 49.3 SiO2
Conrad:
0.333 Na2O 0.667 BaO 0.667 B2O3 0.200 Al2O3 3.07 SiO2
IMC:
% 5.5 Na2O 27.4 BaO 12.4 B2O3 5.4 Al2O3 49.3 SiO2
0.33 Na2O 0.67 BaO 0.67 B2O3 0.20 Al2O3 3.07 SiO2
| |
|