GURUSHAKTI@AOL.COM wrote:

> Has anyone found out if these gerstley substitutes are fritted materials or
> will the glazes with these tend to flocculate like they do with gerstley?
>
> Thanks
> June
>

June,
So far my experience with Laguna Borate is that, while it does settle quite a bit
more than the same glaze with Gerstley Borate, it is much easier to restir than a
traditional fritted glaze.