search  current discussion  categories  kilns & firing - salt & soda 

salt emissions

updated mon 19 jun 00

 

mel jacobson on sun 18 jun 00


many have written a year ago, nils others, that what comes
out of the stack of a salt kiln is salt.

a year ago a fellow wrote a very scientific paper for cm
with the same conclusion.

all of the data is in, proven, but will people listen?
probably not. emotional evidence seems to rule over
science. `my brother in laws friend told me at a party
that chlorine gas comes from the stack and it will kill you. don't
ever get near a salt kiln.` BS

mel


FROM MINNETONKA, MINNESOTA, USA
http://www.pclink.com/melpots (website)