search  current discussion  categories  glazes - cone 8-10 

cone 10 commercial glazes

updated thu 29 jun 00

 

Sarah House on mon 26 jun 00


Hello, could anyone tell me if any companys are making cone 10 glazes? Are
they any good? Please also send contact info for these companys if
possible.
Sarah House

http://www.main.nc.us/wildacres/shouse.pottery.html

GREG MARSHALL on tue 27 jun 00


Sarah,
Laguna Clay Company carries about 30 cone 10 glazes. I've never =
used them so can't give you any information on them. I think the =
distribution center nearest to you would be Laguna-Ohio. You could =
reach them at 740-439-4355.

Greg Marshall

Pamala Browne on tue 27 jun 00


I'm not about to vouch for all of them ,but I have tried and loved Laguna's
^10 blue- brown . Oh ,on white clay ( b-mix,b-mix with sand ) tried it on
soldate and it pin-holed all over the place. Too bad ,too cuz the color was
nice. pamalab



----- Original Message -----
From: Sarah House
To:
Sent: Monday, June 26, 2000 1:28 AM
Subject: cone 10 commercial glazes


> Hello, could anyone tell me if any companys are making cone 10 glazes? Are
> they any good? Please also send contact info for these companys if
> possible.
> Sarah House
>
> http://www.main.nc.us/wildacres/shouse.pottery.html
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>

WHew536674@CS.COM on tue 27 jun 00


Sarah,
Spectrum puts out a line of cone 9/10 glazes. They can be ordered from
Bailey. Their phone # is 1-800-431-6067.
I have used 3 of these, red, pink, salmon, because I was looking for reds in
oxidation. They don't look like a reduction red, but they have even color
consistency and are pretty nice for certain things. Splashed some over a
white glaze that was over a gray slip, and the color broke up and produced a
reduction looking effect, but I haven't played with them too much yet under
or over other glazes. Order a few colors and see how you like them and if
they suit your needs.
Joyce A
Mission, TX

DONALD G. GOLDSOBEL on tue 27 jun 00


Laguna has a slew of cone ten glazes. some of them are holdovers from
Westwood Ceramics. I personally have used their Westwood Chun and Tenmoku
glazes with great success.


Donald 04:28 AM 06/26/2000 -0400, you wrote:
>Hello, could anyone tell me if any companys are making cone 10 glazes? Are
>they any good? Please also send contact info for these companys if
>possible.
>Sarah House
>
>http://www.main.nc.us/wildacres/shouse.pottery.html
>
>___________________________________________________________________________
___
>Send postings to clayart@lsv.ceramics.org
>